Product Details:
Contact Now
Chat Now
|
| Product Name: | Superalloys Nickel Alloy Sheets Incoloy 825 Petrochemical Power Generation | Material: | Nickel Alloy |
|---|---|---|---|
| Grade: | Incoloy 825 | Application: | Oil&gas,aerospace, Petrochemical, And Power Generation Industries |
| Shape: | Sheet,Plate | Specification: | As Per Your Requires |
| Highlight: | Superalloys Nickel Alloy Sheets,Incoloy 925 Nickel Alloy Sheets,Incoloy 825 Sheet |
||
Superalloys Nickel Alloy Sheets Incoloy 825 Petrochemical Power Generation
Incoloy 825 and 925 nickel alloy sheets are specialized materials developed to meet the rigorous demands of the petroleum, chemical, and power generation industries, thanks to their outstanding durability, corrosion resistance, and performance at high temperatures.
Incoloy 825 Sheets:
Incoloy 825 sheets are known for their ability to maintain structural integrity under high temperature and pressure conditions, making them indispensable in applications where durability and reliability are critical. Their high-performance characteristics ensure that they are a preferred choice for challenging industrial applications where standard materials might fail.
| Grade | UNS | Density | Tensile Strength (MPa min) |
Yield Strength (MPa min) |
Reduction of Area ,min (%) | Elongation min (%) | Hardness (HRC) |
| INCOLOY 825 | N08825 | 8.14 | 586MPa min | 241MPa min | / | 30% min | HRC 35max |
Chemical Composition(%):
| INCOLOY 825 | Ni | C | Fe | Mn | Cr | S | Mo |
| 38.0-46.0 | 0.05max | 22.0min | 1.0max | 19.5-23.5 | 0.03max | 2.5-3.5 | |
| Si | Cu | Al | Ti | ||||
| 0.5max | 1.5-3.0 | 0.2max | 0.6-1.2 |
![]()
Contact Person: Alice He
Tel: 0086-19067103413