Automotive Industry Superalloys Incoloy A286 Nickel Alloys Round Bar Rods
Austenitic superalloy A286 can be hardened and strengthened by heat treatment and is used for applications at temperatures up to 1300° F. A286 stainless can also be used for lower stress applications at higher temperatures.
Common Trade Names:
Incoloy A-286 , Nickel Alloy A286 , GH2132 , UNS S66286 , W.Nr 1.4980,
Cronifer 1525 Ti, Superimphy 286, Pyromet A286 , Udimet A286,Grade 660A
Specifications:
AMS 5731, AMS 5734, AMS 5737, AMS 5853, ASTM A453, BS HR 52, BS HR 650, ISO 15156-3 (NACE MR 0175)
Incoloy A-286 Characteristic
Corrosion resistance
INCOLOY A-286's nickel and chromium content provides corrosion resistance and antioxidant properties. The alloy has excellent oxidation resistance at service temperatures up to approximately 1300°F (700°C).
| Grade | UNS | Density |
Tensile Strength |
Yield Strength |
Reduction of Area ,min (%) |
Elongation min (%) |
Hardness (HRC) |
|
INCOLOY A-286 |
S66286 | 7.94 | 895MPa min | 585MPa min | 18% | 15% min | HRC 24-37 |
Chemical Composition(%):
| INCOLOY A-286 | Ni | Cr | Fe | C | Mn | S | Si |
| 24.0-27.0 | 13.5-16.0 | Remainder | 0.08max | 2.0max | 0.03max | 1.0max | |
| B | P | Mo | Ti | Al | V | ||
| 0.001-0.1 | 0.04max | 1.0-1.5 | 1.9-2.35 | 0.35max | 0.1-0.5 |