Home ProductsNickel Alloy Forging Bar

Austenitic Superalloys Incoloy A286 Nickel Alloy Round Bar Rod For Automotive Industry

I'm Online Chat Now

Austenitic Superalloys Incoloy A286 Nickel Alloy Round Bar Rod For Automotive Industry

Austenitic Superalloys Incoloy A286 Nickel Alloy Round Bar Rod For Automotive Industry
Austenitic Superalloys Incoloy A286 Nickel Alloy Round Bar Rod For Automotive Industry Austenitic Superalloys Incoloy A286 Nickel Alloy Round Bar Rod For Automotive Industry

Large Image :  Austenitic Superalloys Incoloy A286 Nickel Alloy Round Bar Rod For Automotive Industry

Product Details:
Place of Origin: China
Brand Name: DINGSCO
Certification: ISO 9001:2015,PED 2014/68/EU,API 6A,API-20B,TSG,NORSOK
Model Number: According to customers' requirements
Payment & Shipping Terms:
Minimum Order Quantity: Negotiable
Price: Negotiable
Packaging Details: According to customers' requests
Delivery Time: (Sample order) 7 days
Payment Terms: T/T
Supply Ability: Negotiable
Contact Now Chat Now

Austenitic Superalloys Incoloy A286 Nickel Alloy Round Bar Rod For Automotive Industry

Description
Product Name: Automotive Industry Austenitic Superalloys Incoloy A286 Nickel Alloys Round Bar Rods Size: Customized
Application: Aerospace,Automotive Material: Nickel Alloy
Grade: Nickel Alloy INCOLOY A-186 Type: Forging Bars
UNS: S66286 Shape: Bar, As Per Your Requirements
Highlight:

Incoloy A286 Rod

,

Incoloy A286 Bar

,

Nickel Alloy Round Bar Rod

Automotive Industry Superalloys Incoloy A286 Nickel Alloys Round Bar Rods
 
Austenitic superalloy A286 can be hardened and strengthened by heat treatment and is used for applications at temperatures up to 1300° F. A286 stainless can also be used for lower stress applications at higher temperatures.
 

Common Trade Names:
Incoloy A-286 , Nickel Alloy A286 , GH2132 , UNS S66286 , W.Nr 1.4980,

Cronifer 1525 Ti, Superimphy 286, Pyromet A286 , Udimet A286,Grade 660A

 

Specifications:
AMS 5731, AMS 5734, AMS 5737, AMS 5853, ASTM A453, BS HR 52, BS HR 650, ISO 15156-3 (NACE MR 0175)

 

Incoloy A-286 Characteristic

  • It is an alloy material with high temperature strength and high temperature oxidation resistance.
  • It has high yield strength, endurance and creep strength below 650°CC
  • It has good processing plasticity and satisfactory welding performance.


Corrosion resistance

INCOLOY A-286's nickel and chromium content provides corrosion resistance and antioxidant properties. The alloy has excellent oxidation resistance at service temperatures up to approximately 1300°F (700°C).

 

Grade UNS Density

Tensile Strength
(MPa min)

  Yield Strength 
(MPa min)

Reduction of Area ,min (%)

Elongation       min (%)

   Hardness    (HRC)

INCOLOY A-286

S66286 7.94 895MPa min 585MPa min 18% 15% min HRC 24-37

 
Chemical Composition(%):
 

INCOLOY A-286 Ni Cr Fe C Mn S Si
24.0-27.0 13.5-16.0 Remainder 0.08max 2.0max 0.03max 1.0max
B P Mo Ti Al V  
0.001-0.1 0.04max 1.0-1.5 1.9-2.35 0.35max 0.1-0.5  

 
 
Application :
 
 
Austenitic Superalloys Incoloy A286 Nickel Alloy Round Bar Rod For Automotive Industry 0
 

Contact Details
Hunan Dinghan New Material Technology Co., LTD

Contact Person: Alice He

Tel: 0086-19067103413

Send your inquiry directly to us (0 / 3000)